With the development of The Times and the progress of science and technology, people have higher and higher requirements for the quantity and quality of industrial products, and the contradiction between the traditional detection technology and the rapid development of industrial requirements is becoming increasingly prominent.  Glass bottles as a kind of packaging supplies, it’s popular because of its good air tightness, clean health, high chemical stability, low cost, recyclable characteristics, has been widely used in food, medicine, cosmetics, drinks, chemical products and other packaging.  People's Daily life cannot leave the glass bottle, the glass bottle production occupies an important position in the national economy.  The bottle must be tested before the production of skin care pharmaceutical beverage filling, such as eliminating unqualified products, and then packaging. In the production process of glass bottle, there will be cracks, bubbles and other defects.


glass material dropping


So where do these defects come from, let’s find out!


1.      When the glass blank falls into the initial mold, it cannot enter the initial mold accurately, and the excessive friction between the blank and the mold wall, resulting in folds. After blowing, the wrinkles spread and enlarge, forming folds in the glass bottle body.


2.       Some feeding machine cutting scar is too large, some glass bottle after molding cutting scar appeared in the bottle body.


3.       The initial mold and molding material of glass bottle are poor, with the lower density, and the oxidation is too fast after high temperature, forming small concave points on the surface of the mold, resulting in the glass bottle surface after molding is not smooth and clean.


4.       Poor quality of glass bottle mold oil will cause the low mold lubrication, the dropping speed will be reduced accordingly, lead to the material change too fast.  


5.       The initial mold design is unreasonable, the mold cavity size is uneven, after the material drops into the forming mold, the blowing diffusion is unevenly spread, causing spots on the glass bottle.


6.      The uneven drip speed of the machine and the Improper adjustment of the nozzle will make the glass bottle initial mold and finished mold temperature is not coordinated, easy to cause cold spots in the glass bottle body, directly affect the finish. 


7.       If the glass material liquid in the kiln is not clean or the material temperature is different, small particles will also appear in the glass bottles.


8.        If the speed of the machine is too fast or too slow, there will be uneven glass bottle body, and the thickness of the bottle wall will be different, resulting in speckles. 


We will eliminate the above defects, Panyue insist on providing customers with every perfect bottle.  Since 2006, we are most proud that we have never received any complaints about quality problems. 


We always believe:The best quality, The best profit.

If you are looking for the cosmetic skincare glass bottle, contact us is the best choice for the progress! 


frosted brown glass bottle for serum lotion oil


Leave A Message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Home

Products

skype

whatsapp